Hastelloy Alloy C22/C276 Fasteners Specifications
Standard |
DIN, ASTM, BS and all International Standards |
Specification |
ASTM / ASME A/SA 193 / 194 IS: 1364, 1367, 3757, 6639, 3640 |
Grade |
Hastelloy C22 (UNS N06022), C276((UNS N10276))
|
Werkstoff Nr |
Hastelloy C22 - 2.4602
Hastelloy C276 - 2.4819
|
Size |
M4 To M100, 3/8" Unc Till 4" UNC |
Length |
UPTO 1 METERS |
Types |
Nuts, Bolts, Screws, Sockets, Studs, Screw, Hex Set Screw, Socket Screw, Cap Screw, Pan Head Screw, Machine Screw, Socket Head Cap Screw, Allen Cap screw, Wing Screw, Washers, Spring Washers, Studs, Anchors, Marine Anchors, Nut, Hexagon Nut, Hex Nut, Hex Coupling Nut, Hex Domed Cap Nuts, Square Nut, Stud Bolts, Hex Head Bolts, Socket Hexagon Head Screw Anchor Bolt, U- Bolts, J Bolts, Mushroom Head Square Neck Bolts, T-Head Bolts, Wing Screw, Eye Bolt, Foundation Bolts, Structural Bolts.
|
Chemical Composition of Hastelloy C22
Element
|
Min
|
Max
|
Molybdenum
|
12.5
|
14.5
|
Chromium
|
20.0
|
22.5
|
Iron
|
2.00
|
6.00
|
Tungsten
|
2.50
|
3.50
|
Cobalt
|
--
|
2.50
|
Carbon
|
--
|
0.010
|
Silicon
|
--
|
0.08
|
Manganese
|
--
|
0.50
|
Vanadium
|
--
|
0.35
|
Phosphorus
|
--
|
0.025
|
Sulfur
|
--
|
0.010
|
Chemical Composition of Hastelloy C276
Element
|
Min
|
Max
|
Molybdenum
|
15.0
|
17.0
|
Chromium
|
14.5
|
16.5
|
Iron
|
4.0
|
7.0
|
Tungsten
|
3.0
|
4.5
|
Cobalt
|
--
|
2.50
|
Manganese
|
--
|
2.5
|
Carbon
|
--
|
1.0
|
Vanadium
|
--
|
.01
|
Phosphorus
|
--
|
35 max
|
Sulfur
|
--
|
.04 max
|
Silicon
|
--
|
.03 max
|
Sulfur
|
--
|
.08 max
|
Mechanical Properties
Grade |
Tensile (ksi) |
.2% Yield (ksi) |
Elongation % |
Hardness (HRb) |
C22 |
115 |
55 |
60 |
89 |
C276 |
110 |
52.6 |
62 |
- |
Physical Properties of Hastelloy C22
Density |
0.314 lb/in3 |
Specific Gravity |
8.69 lb/in3 |
Specific Heat (Btu/lb/Deg F - [32-212 Deg F] |
0.1 |
Melting Point (Deg F) |
2550 |
tdermal Conductivity |
70 |
Mean Coeff tdermal Expansion
|
6.9 |
Modulus of Elasticity Tension
|
29.9 |
Physical Properties of Hastelloy C276
Physical Property |
Temp., °F |
British Units |
Temp., °C |
Metric Units |
Density |
72 |
0.321 lb/in.3 |
22 |
8.89 g/cm.3 |
Melting Range |
2415-2500 |
|
1323-1371 |
|
Electrical Resistivity |
75 |
51 microhm-in. |
24 |
1.30 microhm-m |
Mean Coefficient of
Thermal Expansion
|
75-200 |
6.2 microinches/in.-°F |
24-93 |
11.2 x 10-6 m/m•K |
75-400 |
6.7 microinches/in.-°F |
24-204 |
12.0 x 10-6 m/m•K |
75-600 |
7.1 microinches/in.-°F |
24-316 |
12.8 x 10-6 m/m•K |
75-800 |
7.3 microinches/in.-°F |
24-427 |
13.2 x 10-6 m/m•K |
75-1000 |
7.4 microinches/in.-°F |
24-538 |
13.4 x 10-6 m/m•K |
Thermal Conductivity |
-270 |
50 Btu-in./ft.2 hr.-°F |
-168 |
7.2 W/m•K |
-100 |
60 Btu-in./ft.2 hr.-°F |
-73 |
8.6 W/m•K |
0 |
65 Btu-in./ft.2 hr.-°F |
-18 |
9.4 W/m•K |
100 |
71 Btu-in./ft.2 hr.-°F |
38 |
10.2 W/m•K |
200 |
77 Btu-in./ft.2 hr.-°F |
93 |
11.1 W/m•K |
400 |
90 Btu-in./ft.2 hr.-°F |
204 |
13.0 W/m•K |
600 |
104 Btu-in./ft.2 hr.-°F |
316 |
15.0 W/m•K |
800 |
117 Btu-in./ft.2 hr.-°F |
427 |
16.9 W/m•K |
1000 |
132 Btu-in./ft.2 hr.-°F |
538 |
19.0 W/m•K |
Specific Heat
(Calculated)
|
Room |
0.102 Btu/lb.-°F |
Room |
427 J/kg•K |
We Export To Countries
Mumbai, Ahmedabad, Bhopal, Bikaner, Pune, Delhi, Chennai, Visakhapatnam, Mangalore, Nagpur, Bangalore, Kolkata, Siliguri, Assam, Indore, Hyderabad, Surat, Nashik, Cochin, Thane, Faridabad, Rajkot, Aurangabad, Bhavnagar, Ranchi, Coimbatore, Mysore, Salem, Tirupur, Bikaner, Raipur, Bhubaneswar, Bhilai, Ankleshwar, Bhiwandi, Vadodra, Kochi
We Supply To City
Eastern, Europe, Asia, North, America, Western, Europe, Mid, East/Africa, Australia, Central/South, UAE, America, Portugal, Spain, Indonesia, Italy, Angola, Poland, Brazil, Sri, Lanka, Russia, Chile, Singapore, Oman, Venezuela, Costa, Rica, USA, Qatar, Thailand, Canada, Saudi, Arabia, Bahrain, Egypt, Malaysia, Turkey, Mexico, China, Peru, United, States, Nigeria, Jordan, Kuwait, Dubai, Bangkok, Iran, Germany, UK, New, Zealand, Vietnam, South, Africa, Mexico, Kazakhstan
QUICK ENQUIRY