Nickel Alloy 200/201 Buttweld Fittings Specifications
Grades |
Nickel Alloy 200 (UNS No. N02200)
Nickel Alloy 201 (UNS No. N02201)
|
Standard |
ANSI/ASME B16.9, B16.28, MSS-SP-43. |
Specification |
ASTM B 366 / ASME SB 366 |
Size |
½” NB – 48” NB |
Type |
Seamless / ERW / Welded / Fabricated. |
Schedule |
SCH 5 TO SCH XXS. |
Types of Buttweld Fittings
Nickel Alloy Reducers |
Nickel Alloy Concentric Reducers |
Nickel Alloy Tees |
Nickel Alloy Weldolet |
Nickel Alloy Short Stub End |
Nickel Alloy Eccentric Reducers |
Nickel Alloy Elbows |
Nickel Alloy 3D Elbow |
Nickel Alloy Lap Joint Stub End |
Nickel Alloy End Caps |
Nickel Alloy 5D Elbow |
Nickel Alloy 180° SR Return Bends |
Nickel Alloy Elbows |
Nickel Alloy Short Radius Elbow |
Nickel Alloy 45° Elbows |
Nickel Alloy Reducing Elbow |
Nickel Alloy Long Radius Elbow |
Nickel Alloy 180° LR Return Bends |
Nickel Alloy 45° Elbows |
Nickel Alloy Equal Tee |
Nickel Alloy UnEqual Tee |
Nickel Alloy Reducing Tee |
Nickel Alloy 1D Elbow |
Nickel Alloy 1.5D Elbow |
Nickel Alloy Long Stub Ends |
Nickel Alloy 2D Elbow |
Nickel Alloy 6D Elbow |
Chemical Compositions of Nickel Alloy 200/201 Buttweld Fittings
Material / Purity: |
Alloy 200 |
Alloy 201 |
Ni |
99.00 |
99.00 |
Fe |
.40 |
0.40 |
Mn |
0.35 |
0.35 |
Si |
0.35 |
0.35 |
C |
0.15 |
0.02 |
S |
0.01 |
0.01 |
Cu |
0.25 |
0.25 |
Mechanical Properties of Nickel Alloy 200/201 Buttweld Fittings
Nickel Alloy 201 |
Properties
|
Metric
|
Imperial
|
Tensile strength (annealed)
|
403 MPa
|
58500 psi
|
Yield strength (annealed)
|
103 MPa
|
14900 psi
|
Elongation at break (annealed prior to test)
|
50%
|
50%
|
Nickel Alloy 200 |
Properties
|
Metric
|
Imperial
|
Tensile strength (annealed)
|
462 MPa
|
67000 psi
|
Yield strength (annealed)
|
148 MPa
|
21500 psi
|
Elongation at break (annealed prior to test)
|
45%
|
45%
|
Physical Properties of Nickel Alloy 200/201 Buttweld Fittings
Density |
8.902gm/cc |
Melting Point |
1453 oC |
Boiling Point |
2732 oC |
Thermal Conductivity |
0.909 W/cm/K @ 298.2K |
Electrical Resistivity |
6.84 microhm-cm @ 20 |
Electronegativity |
1.8 Paulings |
Specific Heat |
0.106 Cal/g/ K @ 25 |
Heat of Vaporization |
91.0 K-Cal/gm atom at 2732 oC |
Heat of Fusion |
4.20 Cal/gm mole |
We Export To Countries
Mumbai, Ahmedabad, Bhopal, Bikaner, Pune, Delhi, Chennai, Visakhapatnam, Mangalore, Nagpur, Bangalore, Kolkata, Siliguri, Assam, Indore, Hyderabad, Surat, Nashik, Cochin, Thane, Faridabad, Rajkot, Aurangabad, Bhavnagar, Ranchi, Coimbatore, Mysore, Salem, Tirupur, Bikaner, Raipur, Bhubaneswar, Bhilai, Ankleshwar, Bhiwandi, Vadodra, Kochi
We Supply To City
Eastern, Europe, Asia, North, America, Western, Europe, Mid, East/Africa, Australia, Central/South, UAE, America, Portugal, Spain, Indonesia, Italy, Angola, Poland, Brazil, Sri, Lanka, Russia, Chile, Singapore, Oman, Venezuela, Costa, Rica, USA, Qatar, Thailand, Canada, Saudi, Arabia, Bahrain, Egypt, Malaysia, Turkey, Mexico, China, Peru, United, States, Nigeria, Jordan, Kuwait, Dubai, Bangkok, Iran, Germany, UK, New, Zealand, Vietnam, South, Africa, Mexico, Kazakhstan
QUICK ENQUIRY